Technical Specifications
Download DatasheetNi (Balance), Cr 20.5–23.0, Fe 17.0–20.0, Mo 8.0–10.0, Co 0.5–2.4, W 0.2–1.0, Si ≤ 1.0, Mn ≤ 1.0 (GB/T 14992-2005)
15–53 µm (GB/T 19077-2016)
~ 8.2 g/cm³ (GB/T 3850-2015)
> 99.9% (GB/T 3850-2015)
≥ 6 µm (GB/T 40389-2021)
590 ± 100 MPa (GB/T 228.1-2015)
750 ± 120 MPa (GB/T 228.1-2015)
34 ± 12 % (GB/T 228.1-2015)
330 ± 50 MPa (GB/T 228.1-2015)
710 ± 50 MPa (GB/T 228.1-2015)
45 ± 6 % (GB/T 228.1-2015)
30 Minutes at 600 °C, 70 Minutes at 1,170 °C, Air Cooling
HBD 150, HBD 200, HBD 200Pro, HBD 400, HBD 500, HBD 600, HBD 800, HBD 1600
Besides the listed systems, the material can also be used with third-party systems that meet its requirements. Parameters must be developed separately.
Key Features and Applications
Key Features
- Provides excellent oxidation resistance at high temperature.
- Offers good formability and weldability.
- Is used in hot-section gas turbine parts.
Applications
- Gas turbine combustion chambers and transition ducts.
- Industrial furnace components and heat treatment fixtures.