Technical Specifications
Download DatasheetFe (Balance), Cr 14.0–15.5, Ni 3.5–5.5, Cu 2.5–4.5, Nb 0.15–0.45, Si ≤ 1.0, Mo ≤ 0.5, Mn ≤ 1.0 (GB/T 20878-2007)
15–53 µm (GB/T 19077-2016)
~ 7.7 g/cm³ (GB/T 3850-2015)
> 99.9% (GB/T 3850-2015)
≥ 6 µm (GB/T 40389-2021)
900 ± 100 MPa (GB/T 228.1-2015)
1,150 ± 100 MPa (GB/T 228.1-2015)
14 ± 4 % (GB/T 228.1-2015)
33 ± 3 HRC (GB/T 230.1-2018)
1,050 ± 100 MPa (GB/T 228.1-2015)
1,300 ± 100 MPa (GB/T 228.1-2015)
12 ± 2 % (GB/T 228.1-2015)
36 ± 3 HRC (GB/T 230.1-2018)
270 Minutes at 555 °C, Furnace Cooling
HBD 150, HBD 200, HBD 200Pro, HBD 400, HBD 500, HBD 600, HBD 800, HBD 1600
Besides the listed systems, the material can also be used with third-party systems that meet its requirements. Parameters must be developed separately.
Key Features and Applications
Key Features
- Combines high strength and corrosion resistance.
- Reaches 1,300 MPa tensile strength with heat treatment.
- Single-stage aging makes processing easy.
Applications
- High-strength structural parts for the aerospace and energy sectors.
- Valve and pump components operating in corrosive environments.